Product category
View History
Your Position: Home > Stainless Steel Wire,Stainless iron > Cold Heading Wire > SUS304HC1 Stainless Steel Cold Heading Wires,stainless CHQ wire

SUS304HC1 Stainless Steel Cold Heading Wires,stainless CHQ wire

 

Stainless Steel Cold Heading Wires
CREATION  manufacturers high quality stainless steel cold heading quality (CHQ) wire for production of various types of fasteners.
Grades SUSXM7, 302HQ, 305,305J1, SUS304HC,304HC1,304HC2,304HC3,304HCM, SUS316, SUS3161Cu,SUS410,SUS 430, SUS420,201 (3%Ni), 204Cu, 201Cu,D665,D667,D668
Size Range  0.40mm to 16.00 mm
Condition 1 .00 mm to 1 0.00 mm in Soft Annealed
1.00 mm to 1 6.00 mm in Soap Drawn Skin Pass
Packing Coils of 150 to 400 Kgs in Soft Annealed condition.
Coils of 200 to 500 Kgs in Coated condition.
Stretch + HDPE Wrapped Loose Coils as well as on metal carriers as per customer's requirement.
We are using high quality imported coating salts and drawing lubricants which are free from hazardous substances.
Application Bolts, Nuts, Screws, Rivets, Nails, Automotive lndustries etc.
   
Enquiries & Orders
Please provide following information while forwarding your enquires and orders :
A:Size
B:Grade (as per international standards) with any change from standard composition. Finish condition, tensile strength and surface finish
C:End application
D:Quantity for each size and each grade
E:Delivery Schedule
F:Packaging requirements - coil, spool etc. with specific dimensions
G:Port of shipment / Destination

 

牌号Grade 化学成分Chemical Composition %
C Si Mn P S Ni Cr Mo Cu Other
SUS305 ≤0.12 ≤1.00 ≤2.00 ≤0.045 ≤0.03 10.50-13.00 17.00-19.00 - - -
SUS305J1 ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 11.00-13.50 16.50-19.00 - - -
SUSXM7 ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 8.50-10.50 17.00-19.00 - 3.00-4.00 -
302HQ ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 8.50-10.50 17.00-19.00 - 3.00-4.00 -
SUS430 ≤0.12 ≤0.75 ≤1.00 ≤0.040 ≤0.03 ≤0.6 16.00-18.00 - - -
SUS420 0.16-0.25 1.00 1.00 0.04 0.03 - 12.0-14.0 - - -
SUS410 ≤0.15 ≤1.00 ≤1.00 ≤0.040 ≤0.03 ≤0.60 11.50-13.00 - - -
SUS304HC ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 8.0-10.5 17.0-19.0 - 1.0-3.0 -
SUS304HC1 0.06 0.75 2.0 0.045 0.015 8-10 18-20 - 1.0-1.6 -
SUS304HC2 0.05 1 2.0 0.035 0.02 8-9 17-19 - 2.0-3.0 -
SUS304HC3 0.05 0.75 2.0 0.045 0.015 8-9 18-20 - 3.0-3.5 -
SUS304HCM ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.03 8.0-10.5 17.0-19.0   2.5-4.0  
201CU 0.06 0.75 6-10 0.04 0.015 4.0-5.0 13-17 - 2.0-3.0 -
201CU 0.08 0.75 8-9 0.045 0.015 4.0-5.0 16-18 - 1.0-1.5 -
316LCU 0.03 0.75 2.0 0.04 0.015 10.5-13.5 16.5-18 2.0-3.0 2.0-3.0 -
D667 0.05-0.1 0.6 12-14 0.045 0.015 0.8-1.2 12.5-14.0 - 2.0-3.0 -
D668 0.03-0.06 0.6 12-14 0.045 0.015 1.6-2.5 12.5-13.5 - 1.5-2.0 N0.1≤
D665 0.1 0.75 12-14 0.045 0.015 0.7-1.0 13-14 - 1.5-2.0 -
 

© 1992-2019 China Cold Heading Wire,CHQ Wire,Shanghai Creation Industry Co.,Ltd Copyright, All Rights Reserved.
Anhui Company ADD:No.1818, Xici Liulu, Xinwu High-tech Industrial Development Zone,Wuhu City Anhui Province China (241100),TEL:+86 553 8136866 8136166 FAX:+86 553 8136066,Shanghai Company ADD:No.233 Xinjiang Baihe Town Qingpu District Shanghai, China (201709) FAX:+86 21 5370 0637 Tel:+86 21 5956 9580 E-mail: kily@chqwire.net
QQ 5105013 Skypekilyxsh