China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213

China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213
China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213 China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213 China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213
Usage adapted for all kinds of low intension standard-part and nonstandard -part,
Size 0.08-40mm
Material SWRCH 8A SAE1008A

Characteristics:adapted for all kinds of low intension standard-part and nonstandard -part.
Use of Products:Steel ML08Al,SAE1010,SWRCH8A,C8C,1.0213, are the common using steels produced the Fasteners of low intension and big deformation and the nonstandard-part. The productions have advantages of steady composition, low harmful element, high pure steel and small surface defect. Using them, it is unnecessary to heat treatment and the rate craze of cold forging is low. They are used in the industry of family electricity, traffic, mechanism and transport.

钢号

化学成份%

JIS 标准

SAE 标准

C

Si

Mn

P

S

Al

SWRCH 6A

1006A

0.08 Max

0.10 Max

0.60 Max

0.030 Max

0.035 Max

0.020 Min

SWRCH 8A

1008A

0.10 Max

SWRCH 10A

1010A

0.080.13

0.30~0.60

SWRCH 12A

1012A

0.10~0.15

SWRCH 15A

1015A

0.13~0.18

SWRCH 16A

1016A

0.60~0.90

SWRCH 18A

1018A

0.15~0.20

SWRCH 19A

1019A

0.70~1.00

SWRCH 20A

1020A

0.15~0.20

0.30~0.60

SWRCH 22A

1022A

0.70~1.00

SWRCH 10K

1010K

0.080.13

0.100.35

0.300.60

0.030 Max

0.035 Max

-

SWRCH 12K

1012K

0.100.15

SWRCH 15K

1015K

0.130.18

SWRCH 16K

1016K

0.600.90

SWRCH 17K

1017K

0.150.20

0.300.60

SWRCH 18K

1018K

0.600.90

SWRCH 20K

1020K

0.180.23

0.300.60

SWRCH 22K

1022K

0.70~1.00

SWRCH 24K

1024K

0.190.25

1.35~1.65

SWRCH 25K

1025K

0.220.28

0.30~0.60

SWRCH 27K

1027K

0.220.29

1.20~1.50

SWRCH 30K

1030K

0.270.33

0.60~0.90

SWRCH 33K

1033K

0.300.36

SWRCH 35K

1035K

0.320.38

SWRCH 38K

1038K

0.350.41

SWRCH 40K

1040K

0.370.43

SWRCH 41K

1041K

0.360.44

1.35~1.65

SWRCH 43K

1043K

0.400.46

0.60~0.90

SWRCH 45K

1045K

0.420.48

SWRCH 48K

1048K

0.450.51

SWRCH 50K

1050K

0.470.53

© 1992-2019 China Cold Heading Wire,CHQ Wire,Shanghai Creation Industry Co.,Ltd Copyright, All Rights Reserved.
Anhui Company ADD:No.1818, Xici Liulu, Xinwu High-tech Industrial Development Zone,Wuhu City Anhui Province China (241100),TEL:+86 553 8136866 8136166 FAX:+86 553 8136066,Shanghai Company ADD:No.233 Xinjiang Baihe Town Qingpu District Shanghai, China (201709) FAX:+86 21 5370 0637 Tel:+86 21 5956 9580 E-mail: kily@chqwire.net
QQ 5105013 Skypekilyxsh
ICP:沪ICP备10003366号