Product category
View History
Your Position: Home > Cold Heading Wire,Carbon Steel Wire > Low-carbon steel wire rod Cold Heading And Cold Forging > China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213

China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213

China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213
China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213 China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213 China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213 China Cold heading quality wires, CHQ Wire rod, Cold Forming Wire,Direct Drawing(Hard Drawing)wires,ML08Al,SAE1010,SWRCH8A,C8C,1.0213
Usage adapted for all kinds of low intension standard-part and nonstandard -part,
Size 0.08-40mm
Material SWRCH10A SAE1010A

Characteristics:adapted for all kinds of low intension standard-part and nonstandard -part.
Use of Products:Steel ML08Al,SAE1010,SWRCH8A,C8C,1.0213,are the common using steels produced the Fasteners of low intension and big deformation and the nonstandard-part. The productions have advantages of steady composition, low harmful element, high pure steel and small surface defect. Using them, it is unnecessary to heat treatment and the rate craze of cold forging is low. They are used in the industry of family electricity, traffic, mechanism and transport.

钢号 Grade 化学成份(Chemical composition%
C Si Mn P S Cr Mo B Alt 其他
ML04AL 0.06 0.10 0.20~0.40 0.035 0.035 ~ ~ ~ 0.020 ~
Ml08Al 0.05~0.10 0.30~0.60
ML10Al 0.08~0.13
ML15AL 0.13~0.18
ML15 0.15~0.35 ~
ML20Al 0.18~0.23 0.10 0.020
ML20 0.15~0.35 ~
ML18Mn 0.15~0.20 0.10 0.60~0.90 0.30 0.020
ML22Mn 0.18~0.23 0.70~1.00 0.035
ML20Cr 0.17~0.23 0.30 0.60~0.90 0.90~1.20
ML25 0.22~0.29 0.20 0.30~0.60 ~ ~
ML30 0.27~0.34
ML35 0.32~0.39
ML40 0.37~0.44
ML45 0.42~0.50
ML15Mn 0.14~0.20 0.20~0.40 1.20~1.60
ML25Mn 0.22~0.29 0.25 0.60~0.90
ML30Mn 0.27~0.34
ML35Mn 0.32~0.39
ML37Cr 0.34~0.41 0.90~1.20
ML40Cr 0.38~0.45 0.30 0.90~1.20
ML30CrMo 0.26~0.34 0.80~1.10 0.15~0.25
ML35CrMo 0.32~0.40
ML42CrMo 0.38~0.45 0.90~1.20
ML20B 0.17~0.24 0.40 0.50~0.80 ~ ~ 0.0005~.00035 0.020
ML28B 0.25~0.32 0.60~0.90
ML35B 0.32~0.39 0.50~0.8
ML15MnB 0.14~0.20 0.30 1.20~1.60
ML20MnB 0.17~0.24 0.40 0.80~1.20
ML35MnB 0.32~0.39 1.10~1.40
ML37CrB 0.34~0.41 0.50~0.80 Cr0.20~0.40
ML20MnTiB 0.19~0.24 0.30 1.30~0.60 Ti0.40~0.10
ML15MnVB 0.13~0.18 1.20~160 V0.07~0.12
ML20MnVB 0.19~0.24

使用范围:适用于生产各种低强度级别的标准件和非标件。
产品介绍:ML08Al,SAE1010,SWRCH8A,C8C,1.0213,冷镦钢是生产低强度级别、大变形量紧固件和非标零件的常用钢种,产品具有成分稳定、有害元素低、钢质纯净度高、表面缺陷少等优点,通常使用时不需要热处理、冷镦开裂率低,可用于家电、交通、机械和运输等行业应用。 产品使用: 适用于生产各种低强度级别的标准件和非标件。


钢号 Grade 化学成份(Chemical composition%
C Si Mn P S Cr Mo B Alt 其他
ML04AL 0.06 0.10 0.20~0.40 0.035 0.035 ~ ~ ~ 0.020 ~
Ml08Al 0.05~0.10 0.30~0.60
ML10Al 0.08~0.13
ML15AL 0.13~0.18
ML15 0.15~0.35 ~
ML20Al 0.18~0.23 0.10 0.020
ML20 0.15~0.35 ~
ML18Mn 0.15~0.20 0.10 0.60~0.90 0.30 0.020
ML22Mn 0.18~0.23 0.70~1.00 0.035
ML20Cr 0.17~0.23 0.30 0.60~0.90 0.90~1.20
ML25 0.22~0.29 0.20 0.30~0.60 ~ ~
ML30 0.27~0.34
ML35 0.32~0.39
ML40 0.37~0.44
ML45 0.42~0.50
ML15Mn 0.14~0.20 0.20~0.40 1.20~1.60
ML25Mn 0.22~0.29 0.25 0.60~0.90
ML30Mn 0.27~0.34
ML35Mn 0.32~0.39
ML37Cr 0.34~0.41 0.90~1.20
ML40Cr 0.38~0.45 0.30 0.90~1.20
ML30CrMo 0.26~0.34 0.80~1.10 0.15~0.25
ML35CrMo 0.32~0.40
ML42CrMo 0.38~0.45 0.90~1.20
ML20B 0.17~0.24 0.40 0.50~0.80 ~ ~ 0.0005~.00035 0.020
ML28B 0.25~0.32 0.60~0.90
ML35B 0.32~0.39 0.50~0.8
ML15MnB 0.14~0.20 0.30 1.20~1.60
ML20MnB 0.17~0.24 0.40 0.80~1.20
ML35MnB 0.32~0.39 1.10~1.40
ML37CrB 0.34~0.41 0.50~0.80 Cr0.20~0.40
ML20MnTiB 0.19~0.24 0.30 1.30~0.60 Ti0.40~0.10
ML15MnVB 0.13~0.18 1.20~160 V0.07~0.12
ML20MnVB 0.19~0.24
© 1992-2019 China Cold Heading Wire,CHQ Wire,Shanghai Creation Industry Co.,Ltd Copyright, All Rights Reserved.
Anhui Company ADD:No.1818, Xici Liulu, Xinwu High-tech Industrial Development Zone,Wuhu City Anhui Province China (241100),TEL:+86 553 8136866 8136166 FAX:+86 553 8136066,Shanghai Company ADD:No.233 Xinjiang Baihe Town Qingpu District Shanghai, China (201709) FAX:+86 21 5370 0637 Tel:+86 21 5956 9580 E-mail: kily@chqwire.net
QQ 5105013 Skypekilyxsh
ICP:沪ICP备10003366号