Your Position: Home > Stainless Steel Wire,Stainless iron > EPQ Wire > China Electro Polishing Quality (EPQ)Wire

China Electro Polishing Quality (EPQ)Wire

1   Characteristics
  • Material: Types of 304, 316, 430, 410
  • Size ranges: 1mm to 12mm diameter.
Application
With bright surface, slight magnetism and no cracks in forming, it is widely used in manufacturing bicycle fittings, kitchen and sanitation tools, goods shelf, pet cages, grill racks, decorative handles and baskets, food and medical machinery accessories, etc.
Producing Procedure
Wire produced for final electropolishing of fabricated baskets, racks and other formed parts is referred to as EPQ. This wire has special surface characteristics that result in a very lustrous appearance when electropolished. This procedure is performed by dipping the subject part in a suitable electrolyte and applying a mild electric current, which is the opposite of plating. Small particles of stainless steel are stripped away from the surface until approximately 20 or more microns per side or 0.0015" or more has been removed from the wire surface. The resultant near mirror finish leaves a very smooth, clean and bright cosmetic appearance, while also removing any telltale signs of tack welding or heat tint from parts fabrication.

© 1992-2019 China Cold Heading Wire,CHQ Wire,Shanghai Creation Industry Co.,Ltd Copyright, All Rights Reserved.
Anhui Company ADD:No.1818, Xici Liulu, Xinwu High-tech Industrial Development Zone,Wuhu City Anhui Province China (241100),TEL:+86 553 8136866 8136166 FAX:+86 553 8136066,Shanghai Company ADD:No.233 Xinjiang Baihe Town Qingpu District Shanghai, China (201709) FAX:+86 21 5370 0637 Tel:+86 21 5956 9580 E-mail: kily@chqwire.net
QQ 5105013 Skypekilyxsh
ICP:沪ICP备10003366号