Characteristics
  • Material: Types of 304; 316; 310S; 314; 321; 420.
  • Diameter: 0.8~8.0mm
Application
It can be used in weaving general cloth, mesh , nets, heat resistance belts which are widely used in chemical, food processing, petroleum, kitchen utensils, paper and pulp and conveyer belt industries.

© 1992-2019 China Cold Heading Wire,CHQ Wire,Shanghai Creation Industry Co.,Ltd Copyright, All Rights Reserved.
Anhui Company ADD:No.1818, Xici Liulu, Xinwu High-tech Industrial Development Zone,Wuhu City Anhui Province China (241100),TEL:+86 553 8136866 8136166 FAX:+86 553 8136066,Shanghai Company ADD:No.233 Xinjiang Baihe Town Qingpu District Shanghai, China (201709) FAX:+86 21 5370 0637 Tel:+86 21 5956 9580 E-mail: kily@chqwire.net