Lashing Wire >
1Cr17 Stainless Steel Lashing Wire,China Stainless Steel Lashing WireUsage | 304, 316, 304H, Fruit and vegetable garden wattles, Protectin wattled walls, tying insulation around piping, fastening cable, |
Material | 1Cr17 |
Size | 0.038",0.045",0.062",0.065"英寸 |
Stainless Steel Lashing Wire is used to "lash" an overhead or "aerial" cable or wire to a supporting strand. CREATION & Company produces the highest quality Stainless Steel Lashing Wire available in a variety of materials for the telecommunications, utilities, and Cable TV industries.
• A specially controlled annealing process yields a uniform,fine grain structure throughout wire length and cross section for best results• The Creation lashing wire is packaged as 6 coils per carton for your ordering convenience• Is available in a 430, 302, and 316 stainless steel alloy
No matter what your application or alloy, we can supply you with exactly what you need. Full chemical and mechanical certifications are available with every shipment of lashing wire.
REA ACCEPTANCE
INVENTORY
Stainless Lashing Wire items manufactured by CREATION & Company, Inc. have been accepted and included in the REA list of materials. (Rural Electrification Administration, U.S. Dept. of Agriculture). We stock thousands of pounds of pre-packaged Stainless Lashing Wire available for shipment at the time of order. Call a CREATION & Company Product Manager to discuss alloy and package availability.
PACKAGING
Standard packaging is intended for use with commercial lashers such as Class C and D. CREATION & Company, Inc. stocks straight hub coils as listed below. We offer tapered hub coils as well.All CREATION & Company, Inc. lashing wire is packaged with plastic ties. We believe this offers the most consistent package tension. Plastic ties are also the safest and easiest to use when compared with string or wire ties.
• A specially controlled annealing process yields a uniform,fine grain structure throughout wire length and cross section for best results• The CREATION lashing wire is packaged as 6 coils per carton for your ordering convenience• Is available in a430, 1Cr18Ni9, and 316 stainless steel alloy
Type 430 Stainless• Low carbon, 17% chromium wire• Suitable for general use and in ordinary atmospheric exposure• Will acquire only a dark surface stain• Specifically not recommended for use within 25 miles of salt water or industrial operations which emit pollutants
Type 302 Stainless• 18% chromium, 8% nickel analysis• This wire has excellent resistance to corrosion from industrial atmospheres• Its higher tensile strength and breaking load are an added benefit• A .038 in. diameter Type 302 wire provides strength equal to a .045 in. type Z8c17 wire with better ductility (easier bending and unwinding) and better elongation (less chance of wire breakage from stress)
Type 316 Stainless• Modified 18-10 analysis containing approximately 2.5% molybdenum• More resistant to the corrosive action of most chemicals, including chlorides and sulfides, than any other wire• Particularly resistant to pitting and pin hole corrosion of the kind commonly caused by salt spray• Its use provides the best insurance against failure under the most severe atmospheric conditions• All lashing wire is wound in a straight hub configuration to fit all the standard Creation lashers
Buying tip:
When estimating the length of lashing wire required for a cable run, add the following amounts to the length of the run for single lashing.NOTES:
1. Fits standard C, C2, J2 and Apollo Lasher.
2. Fits G Lasher or C2 and J2 with .065 Modification.
3. For B Lasher only.For wire types other than shown above consult the factory.
CHEMISTRY - ADDITIONAL SPECIFICATIONS
(化学元素含量)MAXIMUM
RANGE
C
MN
P
S
SI
CR
NI
MO
Type1Cr17 (UNS-S43000)
0.12
1.00
0.040
.0030
1.00
16.00 / 18.00
Type 302 (UNS-S30400)
0.08
2.00
0.045
0.030
1.00
18.00 / 20.00
8.00 / 10.50
Type 316 (UNS-S31600)
0.08
2.00
0.045
0.030
1.00
16.00 / 18.00
10.00 / 14.00
2.00 / 3.00
Minimum Elongation for all Loos Lashing Wire = 20% in 10." Wires conform to appropriate AISI Type 1Cr17, 302, or 316 Chemistry. Additionally, Loos & Company lashing wire is wax coated per Bell Telephone Laboratories Spec # AT-7153.
LASHING WIRE SPECIFICATIONS
LOOS PART #
TYPE
(牌号)
WIRE DIA.
(尺寸Inch
NOMINAL COIL SIZE
线圈大小
AVERAGE BREAK STRENGTH
抗拉强度
# COILS / BOX
卷/箱
APPROX SHIP WT. / BOX
每箱重量
LBS.
FEET
038SA302LAC
038SA316LAC
045SA1Cr17LAC302 S.S.
316 S.S.
1Cr17 S.S..038"
.038"
.045"6.29
6.29
6.621,600'
1,600'
1,200'115 LBS.
115 LBS.
125 LBS.6
6
637 LBS.
37 LBS.
40 LBS.045SA302LAC
045SA316LAC
065SA1Cr17LAC302 S.S.
316 S.S.
1Cr17 S.S..045"
.045"
.065"6.62
6.62
5.281,200'
1,200'
450'165 LBS.
165 LBS.
245 LBS.6
6
640 LBS.
40 LBS.
32 LBS.065SA430LA6
065SA302LAC
0450S1Cr17LA2430 S.S.
302 S.S.
1Cr17 S.S..065"
.065"
.045"7.62
5.28
12.13650'
450'
2,200'245 LBS.
300 LBS.
125 LBS.6
6
346 LBS.
32 LBS.
37 LBS.APPROXIMATE INTERIOR DIMENSIONS (INCHES)