表C.1 -交货时热处理条件、产品形式和适用要求的组合
| Heat-treatment condition at delivery | Symbo | Products form a | Applicable requirements in cases where the steel concerned has been ordered with reference to the steel names indicated in | ||||||||||
| Wire rod | Bar | Wire | Tables C.2,C.3,C.4, C.5 or C.6 | Tables C.2,C.3,C.4,C.5,C,6,C.Z C.8 or C.9 | Tables C.2,C.3,C.4,C.5,C.6 or C.10 | Optional | |||||||
| As hot-rolled or peeled | +AR or +PE | X | X | X | Chemical compo- sition as speci- fied in Tables C.2 and C.3 | Me- chanical properties as spec- ified in Tables C.4. C.5 and C.6 | Chemical compo- sition as speci- fied in Tables C.2 and C.3 | Me- chanical properties as spec- ified in Tables C.4, C.5 and C.6 | Values for harden- ability according to Tables C.Z C.8 and C.9 | Chemical compo- sition as speci- fied in Tables C.2 and C.3 | Me- chanical properties as spec- ified in Tables C.4. C.5 and C.6 | Mini- mum core hardness and max- imum diameter accord- ing to TableC.10 | Supplementa- ry or special requirements as specified in Annex Eb |
| Cold drawn | +AR +C | — | X | X | |||||||||
| Cold drawn + spheroidized | +AR+C+ AC | — | X | X | |||||||||
| Cold drawn + spheroidized + skin passed | +AR+C +AC +LC | — | X | X | |||||||||
| Spheroidized or spheroidized + peeled | +AC or +AC+PE | X | X | X | |||||||||
| Spheroidized + cold drawn | +AC+C | — | X | X | |||||||||
| Spheroidized+ cold drawn +spheroidized | +AC+C+ AC | X | X | ||||||||||
| Spheroidized + cold drawn +sphe- roidized +skin passed | +AC+C+ AC+LC | X | X | ||||||||||
| Others | Other delivery conditions may be agreed at the time of ordering | ||||||||||||
| a X=applicable,—=not applicable b If agreed at the time of the enquiry and order. | |||||||||||||
2.化学成分
表C.3-调质用含氮合金钢牌号的化学成分(适用于铸造分析)
| Steel name b | % mass fraction | ||||||||||||
| C | Si c | Mn | P | S | Cr d | Mo | B | Cu | |||||
| 17B2 | 0,15 to 0,20 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | 0,0008 to 0,005 | 0,25 | |||||
| 23B2 | 0,20 to 0,25 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | 0,0008 to 0,005 | 0,25 | |||||
| 28B2 | 0,25 to 0,30 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | —— | 0,0008 to 0,005 | 0,25 | ||||
| 33B2 | 0,30 to 0,35 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 38B2 | 0,35 to 0,40 | 0,30 | 0,60 to 0,90 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 23MnB3 | 0,21 to 0,25 | 0,15 | 0,80 to 1,00 | 0,015 | 0,015 | 0,25 to 0,35 | — | 0,0008 to 0,005 | 0,25 | ||||
| 17MnB4 | 0,15 to 0,20 | 0,30 | 0,90 to 1,20 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 20MnB4 | 0,18 to 0,23 | 0,30 | 0,90 to 1,20 | 0,025 | 0,025 | 0,30 | 0,0008 to 0,005 | 0,25 | |||||
| 23MnB4 | 0,20 to 0,25 | 0,30 | 0,90 to 1,20 | 0.025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 27MnB4 | 0,25 to 0,30 | 0,30 | 0,90 to 1,20 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 30MnB4 | 0,27 to 0,32 | 0,30 | 0,80 to 1,10 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 36MnB4 | 0,33 to 0,38 | 0,30 | 0,80 to 1,10 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 20MnB5 | 0,17 to 0,23 | 0,30 | 1,10 to 1,40 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 23MnB5 | 0,20 to 0,26 | 0,30 | 1,10 to 1,40 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 26MnB5 | 0,23 to 0,29 | 0,30 | 1,20 to 1,50 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 34MnB5 | 0,31 to 0,37 | 0,30 | 1,20 to 1,50 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 37MnB5 | 0,35 to 0,40 | 0,30 | 1,15 to 1,45 | 0,025 | 0,025 | 0,30 | — | 0,0008 to 0,005 | 0,25 | ||||
| 30MoB1 | 0,28 to 0,32 | 0,30 | 0,80 to 1,00 | 0,025 | 0,025 | 0,30e | 0,08 to 0,12 | 0,0008 to 0,005 | 0,25 | ||||
| |||||||||||||
3.力学性能
表C.5 -不含B合金钢牌号的机械性能
| Steel name | Diameter | Delivery condition | ||||||
| +AC or +AC+PE | +AC+C+AC | +AC+C+AC+LC | ||||||
| above mm | up to mm | Rm max. MPa | Z min % | Rm max. MPa | Z min. % | Rm max. MPa | Z min. % | |
| 37Mo2 | 2 | 5 | 560 | 61 | 600 | 59 | ||
| 5 | 40 | 570 | 59 | 550 | 61 | 590 | 59 | |
| 38Cr2 | 2 | 5 | 590 | 62 | 630 | 60 | ||
| 5 | 40 | 600 | 60 | 580 | 62 | 620 | 60 | |
| 46Cr2 | 2 | 5 | 610 | 60 | 650 | 58 | ||
| 5 | 40 | 620 | 58 | 600 | 60 | 640 | 58 | |
| 34Cr4 | 2 | 5 | — | — | 570 | 64 | 610 | 62 |
| 5 | 40 | 580 | 62 | 560 | 64 | 600 | 62 | |
| 37Cr4 | 2 | 5 | 580 | 62 | 620 | 60 | ||
| 5 | 40 | 590 | 60 | 570 | 62 | 610 | 60 | |
| 41Cr4 41CrS4 | 2 | 5 | — | — | 610 | 60 | 650 | 58 |
| 5 | 40 | 620 | 58 | 600 | 60 | 640 | 58 | |
| 25CrMo4 25CrMoS4 | 2 | 5 | 570 | 62 | 610 | 60 | ||
| 5 | 40 | 580 | 60 | 560 | 62 | 600 | 60 | |
| 34CrMo4 | 2 | 5 | — | — | 590 | 62 | 630 | 60 |
| 5 | 40 | 600 | 60 | 580 | 62 | 620 | 60 | |
| 37CrMo4 | 2 | 5 | 610 | 62 | 650 | 60 | ||
| 5 | 40 | 620 | 60 | 600 | 62 | 640 | 60 | |
| 42CrMo4 42CrMoS4 | 2 | 5 | 620 | 60 | 660 | 58 | ||
| 5 | 40 | 630 | 58 | 610 | 60 | 650 | 58 | |
| 41CrNiMo2 41CrNiMoS2 | 2 | 5 | — | — | 640 | 60 | 680 | 55 |
| 5 | 40 | —— | —— | 640 | 60 | 680 | 55 | |
| 34CrNiMo6 | 2 | 5 | —— | —— | 710 | 60 | 750 | 58 |
| 5 | 40 | 720 | 58 | 700 | 60 | 740 | 58 | |
| 41NiCrMo7-3-2 | 2 | 5 | — | — | 710 | 60 | 750 | 58 |
| 5 | 40 | 720 | 58 | 700 | 60 | 740 | 58 | |
4.硬化性要求
表C.7-具有指定(正常)硬化性(+H级)的不含B钢牌号的硬度极限
| Steel name | Sym- bol | Austenitizing temperature °℃±5℃ | Limits of range | Hardness HRC at a distance from quenched end of test piece(in mm) of | |||||||||||||||
| 1 | 2 | 3 | 4 | 5 | 6 | 7 | 8 | 9 | 10 | 11 | 13 | 15 | 20 | 25 | 30 | ||||
| C35EC | +H | 870 | max. | 58 | 57 | 55 | 53 | 49 | 41 | 34 | 31 | 28 | 27 | 26 | 25 | 24 | 23 | 20 | — |
| C35RC | +H | min. | 48 | 40 | 33 | 24 | 22 | 20 | 一 | — | — | ||||||||
| C45EC | +H | 850 | max. | 61 | 60 | 59 | 57 | 53 | 47 | 39 | 34 | 31 | 30 | 29 | 28 | 27 | 26 | 25 | 24 |
| C45RC | +H | min | 51 | 46 | 35 | 27 | 25 | 24 | 23 | 22 | 21 | 20 | — | — | — | — | — | ||
| at a distance from quenched end of test piece(in mm) of | |||||||||||||||||||
| 1,5 | 3 | 5 | 7 | 9 | 11 | 13 | 15 | 20 | 25 | 30 | 35 | 40 | 45 | 50 | |||||
| 37Mo2 | +H | 850 | max. | 59 | 57 | 53 | 47 | 41 | 36 | 32 | 29 | 27 | 25 | — | — | — | — | ||
| min. | 51 | 48 | 41 | 33 | 27 | 26 | 22 | 20 | 一 | ||||||||||
| 38Cr2 | +H | 850 | max. | 59 | 57 | 54 | 49 | 43 | 39 | 37 | 35 | 32 | 30 | 27 | 25 | 24 | 23 | 22 | — |
| min. | 51 | 46 | 37 | 29 | 25 | 22 | 20 | — | |||||||||||
| 46Cr2 | +H | 850 | max. | 63 | 61 | 57 | 52 | 46 | 42 | 40 | 38 | 35 | 33 | 31 | 29 | 28 | 27 | 26 | |
| min | 54 | 49 | 40 | 32 | 28 | 25 | 23 | 22 | 20 | — | |||||||||
| 34Cr4 | +H | 850 | max. | 57 | 57 | 56 | 54 | 52 | 49 | 46 | 44 | 39 | 37 | 35 | 34 | 33 | 32 | 31 | |
| min. | 49 | 48 | 45 | 41 | 35 | 32 | 29 | 27 | 23 | 21 | 20 | — | — | ||||||
| 37Cr4 | +H | 850 | max. | 59 | 59 | 58 | 57 | 55 | 52 | 50 | 48 | 42 | 39 | 37 | 36 | 35 | 34 | 33 | — |
| min. | 51 | 50 | 48 | 44 | 39 | 36 | 33 | 31 | 26 | 24 | 22 | 20 | |||||||
| 41Cr4 | +H | 850 | max. | 61 | 61 | 60 | 59 | 58 | 56 | 54 | 52 | 46 | 42 | 40 | 38 | 37 | 36 | 35 | |
| 41CrS4 | min, | 53 | 52 | 50 | 47 | 41 | 37 | 34 | 32 | 29 | 26 | 23 | 21 | — | — | ||||
| 25CrMo4 | +H | 850 | max. | 52 | 52 | 51 | 50 | 48 | 46 | 43 | 41 | 37 | 35 | 33 | 32 | 31 | 31 | 31 | |
| 25CrMoS4 | min. | 44 | 43 | 40 | 37 | 34 | 32 | 29 | 27 | 23 | 21 | 20 | — | — | 一 | — | |||
| 34CrMo4 | +H | 850 | max. | 57 | 57 | 57 | 56 | 55 | 54 | 53 | 52 | 48 | 45 | 43 | 41 | 40 | 40 | 39 | |
| min. | 49 | 49 | 48 | 45 | 42 | 39 | 36 | 34 | 30 | 28 | 27 | 26 | 25 | 24 | 24 | — | |||
| 37CrMo4 | +H | 850 | max | 60 | 60 | 60 | 59 | 58 | 56 | 55 | 54 | 51 | 48 | 46 | 45 | —— | |||
| min. | 52 | 50 | 49 | 47 | 45 | 43 | 40 | 37 | 34 | 32 | 31 | 30 | |||||||
| 42CrMo4 | +H | 850 | max. | 61 | 61 | 61 | 60 | 60 | 59 | 59 | 58 | 56 | 53 | 51 | 48 | 47 | 46 | 45 | |
| 42CrMoS4 | min | 53 | 53 | 52 | 51 | 49 | 43 | 40 | 37 | 34 | 32 | 31 | 30 | 30 | 29 | 29 | |||