1.化学成分(化学成分)
表1:化学成分,单位%
| 表1 – 化学成分 | ||||||
| 单位 % | ||||||
| 牌号 | C | Si a) | Mn | P | S | B b) |
| SWRCHB223 | 0.20-0.26 | 0.10-0.35 | 0.60-0.90 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB237 | 0.34-0.40 | 0.10-0.35 | 0.60-0.90 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB320 | 0.17-0.23 | 0.10-0.35 | 0.70-1.00 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB323 | 0.20-0.26 | 0.10-0.35 | 0.70-1.00 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB331 | 0.28-0.34 | 0.10-0.35 | 0.70-1.00 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB334 | 0.31-0.37 | 0.10-0.35 | 0.70-1.00 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB420 | 0.17-0.23 | 0.10-0.35 | 0.80-1.10 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB526 | 0.23-0.29 | 0.10-0.35 | 0.90-1.20 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB620 | 0.17-0.23 | 0.10-0.35 | 1.10-1.40 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB623 | 0.20-0.26 | 0.10-0.35 | 1.10-1.40 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB726 | 0.23-0.29 | 0.10-0.35 | 1.20-1.50 | ≤0.030 | ≤0.030 | ≥0.0008 |
| SWRCHB734 | 0.31-0.37 | 0.10-0.35 | 1.20-1.50 | ≤0.030 | ≤0.030 | ≥0.0008 |
本表所列所有钢种均不得超过Cu 0.30%、Ni 0.20%和Cr 0.20%。注a) Si的下限值也可以根据接收当事人之间的协议设定为小于0. 10%的值。(b) B的含量可不低于0.0005%,取决于接收方之间的协议。
2.燃烧性
表 3与淬火端的距离和硬度
| 牌号 | 距淬火端距离 mm | 热处理温度 ℃ | ||||||||||||||||
| 硬度 HRC | 1.5 | 3 | 5 | 7 | 9 | 11 | 13 | 15 | 20 | 25 | 30 | 35 | 40 | 45 | 50 | 正火 | 淬火 | |
| SWRCHB223 | 上限 / 下限 | 50 42 | 49 40 | 48 22 | 46 20 | 41 – | 32 – | 24 – | 21 – | – – | – – | – – | – – | – – | – – | – – | 900 | 875 |
| SWRCHB237 | 上限 / 下限 | 58 50 | 58 47 | 57 37 | 55 26 | 52 21 | 46 – | 38 – | 32 – | 26 – | 24 – | 23 – | 21 – | – – | – – | – – | 870 | 845 |
| SWRCHB320 | 上限 / 下限 | 48 40 | 47 39 | 46 33 | 44 21 | 39 – | 31 – | 26 – | 23 – | – – | – – | – – | – – | – – | – – | – – | 925 | 925 |
| SWRCHB323 | 上限 / 下限 | 50 42 | 49 41 | 48 34 | 46 20 | 42 – | 33 – | 27 – | 23 – | – – | – – | – – | – – | – – | – – | – – | 900 | 870 |
| SWRCHB331 | 上限 / 下限 | 54 46 | 53 45 | 52 39 | 51 23 | 48 – | 36 – | 29 – | 25 – | 20 – | – – | – – | – – | – – | – – | – – | 900 | 870 |
| SWRCHB334 | 上限 / 下限 | 57 49 | 56 48 | 55 45 | 54 30 | 51 21 | 47 – | 39 – | 31 – | 24 – | 22 – | – – | – – | – – | – – | – – | 870 | 845 |
| SWRCHB420 | 上限 / 下限 | 48 40 | 48 38 | 47 32 | 45 22 | 41 – | 35 – | 30 – | 27 – | 22 – | – – | – – | – – | – – | – – | – – | 925 | 925 |
| SWRCHB526 | 上限 / 下限 | 52 44 | 52 43 | 51 40 | 50 28 | 48 21 | 45 – | 41 – | 33 – | 23 – | – – | – – | – – | – – | – – | – – | 900 | 870 |
| SWRCHB620 | 上限 / 下限 | 48 40 | 48 39 | 48 37 | 47 30 | 46 22 | 44 – | 40 – | 36 – | 29 – | 25 – | 21 – | – – | – – | – – | – – | 925 | 925 |
| SWRCHB623 | 上限 / 下限 | 50 42 | 50 41 | 49 39 | 48 35 | 48 27 | 46 20 | 44 – | 41 – | 30 – | 22 – | – – | – – | – – | – – | – – | 900 | 870 |
| SWRCHB726 | 上限 / 下限 | 52 44 | 52 43 | 52 42 | 51 40 | 50 34 | 49 27 | 48 23 | 45 20 | 36 – | 27 – | 23 – | 20 – | – – | – – | – – | 900 | 870 |
| SWRCHB734 | 上限 / 下限 | 57 49 | 56 48 | 56 47 | 55 45 | 55 43 | 54 37 | 53 31 | 51 26 | 43 20 | 33 – | 28 – | 25 – | 22 – | 20 – | – – | 870 | 845 |
3.线材的力学性能。
表4D工艺中线材的机械性能
| D工艺线材力学性能 | |||
| 牌号 | 抗拉强度 N/mm2 | 断面收缩率 % | 硬度 HRB |
| SWCHB 223 | ≤750 | ≥45 | ≤100 |
| SWCHB 320 | |||
| SWCHB 323 | |||
| SWCHB 420 | |||
| SWCHB 526 | |||
| SWCHB 620 |
注1线径为20 mm以上的情况下,光圈为比表2的值减去5的值。另外,对于3 mm以下,光圈没有规定。2 1 N/mm2 = 1 MPa
4.脱煤层深
表 6 平均脱碳层深度允许极限
| 平均脱碳层深度 | ||
| 线径 (mm) | 铁素体脱碳层深度 | 总脱碳层深度 |
| ≤15 | <0.02 | <0.15 |
| 15<d≤25 | <0.03 | <0.20 |
| 25<d≤32 | <0.04 | <0.25 |
在脱碳层深度SWCH 30 K ~ SWCH 50 K的线上,并且有订货者指定的情况下,进行10.3.1的试验,其平均脱碳层深度的容许限度根据表4。然而,对于直径超过32毫米的线,应根据接受方之间的协议进行。
5.线径的容差及偏径差
表 7线径的容差及偏径差
| 表7 线径公差和偏差 | ||
| 单位 mm | ||
| 线径 | 公差 | 偏径差 |
| ≤3 | 0-0.025 | 0.013 |
| 3<d≤6 | 0-0.030 | 0.013 |
| 6<d≤10 | 0-0.036 | 0.013 |
| 10<d≤18 | 0-0.043 | 0.013 |
| 18<d≤30 | 0-0.070 | 0.013 |
| 30<d≤40 | 0-0.100 | 0.013 |
| 40<d≤50 | 0-0.150 | 0.013 |
注(3)偏径差是指线的同一截面中直径的最大值和最小值的差。